Ceramics Studio Ships 12,000 Pieces a Year Without Plastic Film
Customer: a ceramics studio producing hand-thrown stoneware, direct-to-consumer and gallery supply.

Products used: Honeycomb Paper Roll, 30 cm x 100 m, 80 gsm; Cushion Paper Pads for bases.
Result: plastic film eliminated; breakage tracked across four quarters below the pre-change rate, with one persistent failure mode documented.
The starting point
The studio wrapped every piece in plastic film over a foam collar, in a corrugated box. Breakage ran around 2% — acceptable by studio standards, embarrassing by gallery ones. The change was initiated by a gallery partner's packaging policy rather than by the damage rate: the gallery would no longer accept consignments containing plastic film.
The system
Each piece: a base pad (cushion paper, 6 layers, cut to the foot), then two wraps of honeycomb roll with the second wrap run opposite the first, then the box, then a top pad if the lid clearance allowed. Bowls got a third wrap; plates were stacked in pairs with a pad between and wrapped as a unit.
| Parameter | Specification |
|---|---|
| Roll | 30 cm x 100 m, 80 gsm brown |
| Wraps | 2 standard, 3 for bowls |
| Base pads | 6 layers, 1,000 pcs MOQ |
| Packing time | 48 s → 52 s per piece (first quarter) |
Four quarters of breakage
| Quarter | Breakage rate | Notes |
|---|---|---|
| Q1 (transition) | 1.8% | Learning curve on wrap tension |
| Q2 | 1.1% | Wrap pattern standardised |
| Q3 | 0.9% | Pad added under lids of wide bowls |
| Q4 | 0.8% | Stable |
The final rate beat the plastic system — the studio's prior 2% was never purely a material problem, and the discipline of a written wrap pattern improved the human factor as much as the material change did.
The failure mode, documented honestly
Wide, shallow bowls with unglazed feet are the system's weak point. The honeycomb wraps the rim and body well, but under a hard base-first drop the foot ring can shear through two wraps at the contact point. The Q3 fix — a pad folded into the base of the wrap bundle — reduced it but did not eliminate it. The studio's remaining breakage is almost entirely this one failure mode, at 0.8%.
A third wrap would probably close most of the gap. The studio chose not to: the marginal material and time was judged not worth it for a rate that low, and that trade-off is the real lesson — packaging engineering is choosing where to stop.
Data note: figures in this article are representative values from this application type, shown for specification guidance. Project-specific data is available under NDA on request.